Polymer Property : Density = 0.04104 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.136 g/cc
0.04104 lb/in³
ISO 1183
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
Density 1.136 g/cc
0.04104 lb/in³
Melt; ISO 1183
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Density 1.136 g/cc
0.04104 lb/in³
Melt; ISO 1183
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..