Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.119 g/cc | 0.04043 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON AD000 ABS LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive. |