Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.116 - 1.117 g/cc | 0.04032 - 0.04035 lb/in³ | |
Kazanorgsintez Diethyleneglycol Production Method: Obtained by hydrolyzation of ethylene oxide. Application: Intended for organic synthesis industry, as the extractant of aromatic hydrocarbons, for natural gas drying and in some o.. |
|||
Density | 1.116 g/cc | 0.04032 lb/in³ | |
Dow Nordel® IP 4520 Molded Brake Part FormulationNordel® IP 4520 |