Polymer Property : Density = 0.0398 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0398 lb/in³
ASTM D-1475
Lucite International Elvacite ® 2669 Acrylic Resin
Elvacite® 2669, the first in this series, is a solid acrylic bead copolymer which can be dissolved in slightly alkaline aqueous systems. This distinct capability makes the product particularly su..
Density 1.10 g/cc
0.0398 lb/in³
ASTM C134
BNZ Materials Color CA Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..