Polymer Property : Density = 0.03913 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.083 g/cc
0.03913 lb/in³
Dow Nordel® IP 4640 General Purpose Compound
FormulationNordel® IP 4640
Density 1.083 g/cc
0.03913 lb/in³
Dow Nordel® IP 4770P General Purpose Compound
FormulationNordel® IP 4770P
Density 1.083 g/cc
0.03913 lb/in³
Dow Nordel® IP 4770R General Purpose Compound
FormulationNordel® IP 4770R