Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.078 g/cc | 0.03895 lb/in³ | ASTM D4052 |
ExxonMobil Mobil Glygoyle 150 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Density | 1.078 g/cc | 0.03895 lb/in³ | ASTM D4052 |
ExxonMobil Mobil Glygoyle 150 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Density | 1.078 g/cc | 0.03895 lb/in³ | |
BASF Epsilon-Caprolactone Formula: C6H10O2CAS: 502-44-3Description: Epsilon-caprolactone is a colorless to yellow liquid, with a perceptible odor. It is soluble in water.Synonyms: 6-Hydroxyhexanoic acid lactone, Caprolacton.. |