Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.073 g/cc | 0.03876 lb/in³ | |
NEU NeuSoft™ 602-60A Ester TPU / SBC blend |
|||
Density | 1.073 g/cc | 0.03876 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Density | 1.073 g/cc | 0.03876 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific) LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |