Physical Properties Metric English Comments
Density 1.0603 g/cc
0.038306 lb/in³
BASF Lupragen® 106 2,2'-Dimorphalinyldiethylether
Formula: C12H24N2O3CAS: 6425-39-4Description: 2,2’-Dimorpholinyldiethylether is a colorless to yellow liquid, with an amine-like odor. It is also miscible with water.Synonyms: DMDEE, Morpholone 4,..