Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.995 - 1.05 g/cc | 0.0359 - 0.0381 lb/in³ | |
Lord Adhesives 506 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.995 - 1.05 g/cc | 0.0359 - 0.0381 lb/in³ | |
Lord Adhesives 510 Fast Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |