Physical Properties Metric English Comments
Density 1.042 g/cc
0.03764 lb/in³
Pyrotek H-10B Fabric
Ideal covering for high-temperature compressible gaskets.Information provided by Pyrotek.
Density 1.042 g/cc
0.03764 lb/in³
Dow VORALUX™ HL 430 Copolymer Polyol
VORALUX™ HL 430 is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile and filtered to 100 microns. It is used in the manufacture of flexible slabstock polyurethan..