Polymer Property : Density = 0.036738 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.0169 g/cc
0.036738 lb/in³
BASF 1,4-Butanediol (BDO)
Formula: C4H10N2CAS: 110-63-4Description: 1,4-Butanediol (BDO) is a colorless, odorless liquid. It is miscible in all proportions with water and soluble with organic solvent.Synonyms: Butane-1,4-di..