Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.012 g/cc | 0.03656 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON MD000AP PP LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing. |