Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.997 g/cc | 0.0360 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 7301 BLK The data is the actual data obtained from the above sample. This material is based on Shell's Kraton G technology. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.996 g/cc | 0.0360 lb/in³ | |
BASF 3-Hexyne-2,5-diol Formula: C6H10O2OCAS: 3031-66-1Description: 3-Hexyne-2,5-diol is a yellowish liquid or solidified, with a pungent odor. It is miscible in water.Synonyms: Hexin-3-diol-2,5, Hex-3-yne-2,5-diol, Hex-3.. |