Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9706 - 0.9945 g/cc | 0.03507 - 0.03593 lb/in³ | |
Lord Adhesives Flocklok® 853A Flock Adhesive LORD Flocklok® 853A is a blocked, heat-curing, singlecoat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates pro.. |
|||
Density | 0.9706 g/cc | 0.03507 lb/in³ | |
Lord Adhesives Flocklok® 870 Flock Adhesive LORD Flocklok® 870 adhesive is a single-coat adhesive used to adhere polyester or nylon flock if beers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good r.. |