Polymer Property : Density = 0.03251 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.8999 g/cc
0.03251 lb/in³
HPC-3C
Lord Adhesives HPC-3C Fluoroelastomer Coating
LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu..
Density 0.8999 g/cc
0.03251 lb/in³
HPC-3B
Lord Adhesives HPC-3B Fluoroelastomer Coating
LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu..