Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.8678 g/cc | 0.03135 lb/in³ | |
Saint-Gobain Chemfab® 8 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.. |