Physical Properties Metric English Comments
Density 0.8286 g/cc
0.02993 lb/in³
Calculated from weight of 18 oz/sy
Mid-Mountain Materials SILTEX® 18 Amorphous Silica Textile
Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher..