Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.7716 g/cc @Temperature 82.2 °C |
0.02788 lb/in³ @Temperature 180 °F |
ASTM D4052 |
ChevronTexaco Saturating Wax 2 FeaturesChevron Saturating Wax 2 is a food grade blend of fully refined paraffin wax and a wet strength additive. It is specifically formulated to impart moisture resistance and structural strength.. |