Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.689 - 0.753 g/cc | 0.0249 - 0.0272 lb/in³ | |
Engineered Syntactic Systems HZ-45 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |
|||
Density | 0.690 g/cc @Temperature 25.0 °C |
0.0249 lb/in³ @Temperature 77.0 °F |
bulk |
3D Systems DuraForm® AF Nylon for SLS® Systems Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use. For use with all selective laser sintering SLS® systems.ApplicationsHousings and enclosuresCo.. |
|||
Density | 0.690 g/cc | 0.0249 lb/in³ | |
BASF Isopropylamine Formula: C3H9NCAS: 75-31-0Description: Isopropanolamine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisopropanolamin, 1-Amin.. |