Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.663 g/cc | 0.0240 lb/in³ | |
Pyrotek A-5C Fiberglass Fabric Z-5 with proprietary Pyroseal red coating on one side to provide an airtight covering while maintaining flexibility.Information provided by Pyrotek. |