Physical Properties Metric English Comments
Density 0.513 - 0.577 g/cc
0.0185 - 0.0208 lb/in³
Engineered Syntactic Systems AZ-34 Deep Water Syntactic Foam
Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c..