Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0185 g/cc | 0.000668 lb/in³ | 100 rpm |
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave.. |