Physical Properties Metric English Comments
Density >= 0.0184 g/cc
>= 0.000666 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS 33MB Modified Expandable Polystyrene
Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals.
Density >= 0.0184 g/cc
>= 0.000666 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS M77BHD Expandable Polystyrene Resin
Applications Insulation, SIP's, Fabricated PackagingInformation provided by NOVA Chemicals
Density >= 0.0184 g/cc
>= 0.000666 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS M77BHD Modified Expandable Polystyrene
Applications: Insulation, SIP's, fabricated packagingInformation provided by NOVA Chemicals.