Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0176 g/cc | >= 0.000637 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 34RA Regular Expandable Polystyrene Applications: Fabricated packagingInformation provided by NOVA Chemicals. |