Density 0.368 - 0.481 g/cc

@Treatment Temp. 982 °C,
Time 86400 sec
0.0133 - 0.0174 lb/in³

@Treatment Temp. 1800 °F,
Time 24.0 hour
Fired
Unifrax Foamfrax® Isofoam® RG Insulation
Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory..
Density 0.368 - 0.481 g/cc

@Treatment Temp. 982 °C,
Time 86400 sec
0.0133 - 0.0174 lb/in³

@Treatment Temp. 1800 °F,
Time 24.0 hour
Fired
Unifrax Foamfrax® RG Insulation
Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory..
Density 0.368 - 0.481 g/cc

@Treatment Temp. 1260 °C,
Time 86400 sec
0.0133 - 0.0174 lb/in³

@Treatment Temp. 2300 °F,
Time 24.0 hour
Fired
Unifrax Foamfrax® RG Plus Insulation
Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process..
Density 0.417 - 0.481 g/cc
0.0150 - 0.0174 lb/in³
Engineered Syntactic Systems BZ-28 Deep Water Syntactic Foam
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having..