Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.450 g/cc | 0.0163 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ S1006B Polyethylene, Crosslinked (XLPE) Available as Catalyst Masterbatch component for PolyOne Syncure System.Oven Aging values are >75, and were measured on a 95 phr S1025A / 5 phr S1006B Syncure System. Pellet appearance is 1/8 cylindr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | True Density as as measured by gas displacement |
Potters Industries Sphericel® 45P25 Hollow Engineered Glass Microspheres Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
MarkeTech H-4 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |
|||
Density | 0.451 g/cc | 0.0163 lb/in³ | |
Hardwire 12x-4-12 Low Density Tape The 12X Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 12X wire cord is used where the traits of high tensile strain, excellent conformabi.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | ISO 1183 |
Stir SpA POROCELL Z 559 AT (PVC) Application: Matt super foam for injection moldingInformation provided by STIR SpA |
|||
Density | 0.450 - 0.550 g/cc | 0.0163 - 0.0199 lb/in³ | |
Sibur PVC S-6558-U-LP Suspension Polyvinyl Chloride (PVC) For production of plasticized and rigid articles of general purpose. |
|||
Density | 0.450 - 0.550 g/cc | 0.0163 - 0.0199 lb/in³ | |
Sibur PVC S-7058-M Suspension Polyvinyl Chloride (PVC) For production of articles by methods of extrusion, calendaring, pressing, rolling, or molding under pressure. |
|||
Density | 0.450 - 0.550 g/cc | 0.0163 - 0.0199 lb/in³ | |
Sibur PVC S-7059-M Suspension Polyvinyl Chloride (PVC) For production of articles by methods of extrusion, calendaring, pressing, rolling, or molding under pressure. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ 1015 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ 1020R Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ 1040 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ 1060 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1015 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1020 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1040 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1040 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1040H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1060 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1060H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ 1015M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ 1020 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ 1020M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
3M Cushion-Mount™ E1060 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Density | 0.450 - 0.480 g/cc | 0.0163 - 0.0173 lb/in³ | |
Pyrotek AFB-2300 HT Structural Board AFB-2300 HT is a ceramic fiber board which features a unique alumina-based binder. This white board is heat-treated to eliminate all possible out-gassing and withstands temperatures up to 1260°C.H.. |
|||
Density | 0.450 g/cc | 0.0163 lb/in³ | |
Pyrotek LUMIFELT AL20L High Temperature Kevlar® Felt Lumifelt is composed of heat resistant para linked type Kevlar® fiber. Lumifelt is an ideal insulating pad for a variety of applications. It is needle punched to give it high tensile strength and.. |