Physical Properties Metric English Comments
Density 0.0139 g/cc
0.000502 lb/in³
Based on 75 times expansion
Samsung Cheil Industries Starex® SF-100H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0139 g/cc
0.000502 lb/in³
Based on 75 times expansion
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0139 g/cc
0.000502 lb/in³
Based on 75 times expansion
Samsung Cheil Industries Starex® SF-300H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0139 g/cc
0.000502 lb/in³
Based on 75 times expansion
Samsung Cheil Industries Starex® SF-100H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0139 g/cc
0.000502 lb/in³
Based on 75 times expansion
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0139 g/cc
0.000502 lb/in³
Based on 75 times expansion
Samsung Cheil Industries Starex® SF-300H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.