Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.360 g/cc | 0.0130 lb/in³ | Effective density of spheres |
Potters Industries Q-Cel® 6036 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Density | 0.360 g/cc | 0.0130 lb/in³ | Effective Density as measured by liquid displacement |
Potters Industries Q-Cel® 7036 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Density | 0.360 g/cc | 0.0130 lb/in³ | ASTM D1667 |
Saint-Gobain T-Bond II® Semi-Rigid Polyurethane Foam Structural Glazing and Cladding Spacer System Description: Semi-Rigid Polyurethane Foam Substrate used as a Structural Glazing and Cladding Spacer System for In-Shop Fabrication. Semi-Rigid Polyurethane: An open cell structure allows air and mo.. |