Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0128 g/cc | >= 0.000463 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS 33MB Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0128 g/cc | >= 0.000463 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS M77BHD Expandable Polystyrene Resin Applications Insulation, SIP's, Fabricated PackagingInformation provided by NOVA Chemicals |
|||
Density | >= 0.0128 g/cc | >= 0.000463 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS M77BHD Modified Expandable Polystyrene Applications: Insulation, SIP's, fabricated packagingInformation provided by NOVA Chemicals. |