Density 0.336 g/cc
0.0122 lb/in³
Fired Density at 2300°F
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M22 Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..