Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.199 g/cc | 0.00718 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 1/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |