Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.130 - 0.170 g/cc | 0.00470 - 0.00614 lb/in³ | |
3M K15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.130 - 0.170 g/cc | 0.00470 - 0.00614 lb/in³ | |
3M S15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.125 - 0.170 g/cc | 0.00452 - 0.00614 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |