Density 0.149 g/cc
0.00538 lb/in³
Folded
Unifrax Anchor-Loc® 2400 Ceramic Fiber Modules
The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us..
Density 0.149 g/cc
0.00538 lb/in³
Folded
Unifrax Anchor-Loc® 2600 Ceramic Fiber Modules
The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us..
Density 0.149 g/cc
0.00538 lb/in³
Unifrax Fiberwall® Bonded 22 Bonded Module System
Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces..
Density 0.149 g/cc
0.00538 lb/in³
Unifrax Fiberwall® Bonded 26 Bonded Module System
Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces..
Density 0.149 g/cc
0.00538 lb/in³
Unifrax Fiberwall® Bonded 24 Bonded Module System
Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces..