Polymer Property : Density = 0.00332 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0720 - 0.0920 g/cc
0.00260 - 0.00332 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Density 0.0720 - 0.0920 g/cc
0.00260 - 0.00332 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..