Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0513 g/cc | 0.00185 lb/in³ | |
Hexcel® HexWeb® HRP - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.0513 g/cc | 0.00185 lb/in³ | |
Hexcel® HexWeb® HRP/OX - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.0513 g/cc | 0.00185 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 1/8 - 3.2 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |