Density 0.0370 - 0.0490 g/cc
0.00134 - 0.00177 lb/in³
sheet density
Zotefoams Evazote® EV45CN Conductive Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Density 0.0370 - 0.0470 g/cc
0.00134 - 0.00170 lb/in³
sheet density
Zotefoams Plastazote® LD45 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0370 - 0.0470 g/cc
0.00134 - 0.00170 lb/in³
sheet density
Zotefoams Plastazote® LD45IC Low Density Polyethylene Foam, Intermediate Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0370 g/cc
0.00134 lb/in³
Molded density, ASTM D1622
Covestro Bayfill® EA 2001 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.