Physical Properties Metric English Comments
Density 0.0260 - 0.0340 g/cc
0.000939 - 0.00123 lb/in³
sheet density
Zotefoams Plastazote® LD30 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0260 g/cc
0.000939 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam
Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi..