Physical Properties Metric English Comments
Density >= 0.0224 g/cc
>= 0.000810 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS 33MAHD Modified Expandable Polystyrene
Applications: Insulation, board stockInformation provided by NOVA Chemicals.
Density >= 0.0224 g/cc
>= 0.000810 lb/in³
Batch Expansion
NOVA Chemicals EPS 34RCLV Expandable Polystyrene Resin
Applications High Strength/High Density > 1.5pcf Packaging and Produce BoxesInformation provided by NOVA Chemicals
Density >= 0.0224 g/cc
>= 0.000810 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS R244C Expandable Polystyrene Resin
Applications Thermal and Regular PackagingInformation provided by NOVA Chemicals