Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Batch Expansion |
NOVA Chemicals EPS 34RALV Expandable Polystyrene Resin Applications High Strength/High Density > 1.25pcf Packaging and Produce BoxesInformation provided by NOVA Chemicals |
|||
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 34RB Regular Expandable Polystyrene Applications: PackagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Batch Expansion |
NOVA Chemicals EPS 34RBLV Expandable Polystyrene Resin Applications High Strength/High Density > 1.25pcf Packaging and Produce BoxesInformation provided by NOVA Chemicals |
|||
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS M77BLV Expandable Polystyrene Resin Applications Insulation, SIP's, Fabricated PackagingInformation provided by NOVA Chemicals |
|||
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS M77BLV Low Volatile/Low Pentane Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS M77C Expandable Polystyrene Resin Applications Insulation, SIP's, Fabricated Packaging/Fine SurfaceInformation provided by NOVA Chemicals |
|||
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Batch Expansion |
NOVA Chemicals EPS M97BC Low Volatile/Low Pentane Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0192 g/cc | >= 0.000694 lb/in³ | Batch Expansion |
NOVA Chemicals EPS R244C Expandable Polystyrene Resin Applications Thermal and Regular PackagingInformation provided by NOVA Chemicals |