Polymer Property : Density = 0.000578 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0150 - 0.0160 g/cc
0.000542 - 0.000578 lb/in³
IRPC Polimaxx Pentfoam 361F Expandable Polystyrene
GENERAL: PENTFOAM "361F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..