Polymer Property : Density = 0.000434 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.00800 - 0.0120 g/cc
0.000289 - 0.000434 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T243C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
Density 0.00400 - 0.0120 g/cc

@Pressure 0.1013 MPa,
Temperature 20.0 °C
0.000145 - 0.000434 lb/in³

@Pressure 14.69 psi,
Temperature 68.0 °F
BASF Basotect G Foam
Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh..
Density 0.00400 - 0.0120 g/cc

@Pressure 0.1013 MPa,
Temperature 20.0 °C
0.000145 - 0.000434 lb/in³

@Pressure 14.69 psi,
Temperature 68.0 °F
BASF Basotect G+ Foam
Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh..
Density 0.00400 - 0.0120 g/cc

@Pressure 0.1013 MPa,
Temperature 20.0 °C
0.000145 - 0.000434 lb/in³

@Pressure 14.69 psi,
Temperature 68.0 °F
BASF Basotect UF Foam
Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh..
Density 0.00400 - 0.0120 g/cc

@Pressure 0.1013 MPa,
Temperature 20.0 °C
0.000145 - 0.000434 lb/in³

@Pressure 14.69 psi,
Temperature 68.0 °F
BASF Basotect V3012 Foam
Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh..
Density 0.00400 - 0.0120 g/cc

@Pressure 0.1013 MPa,
Temperature 20.0 °C
0.000145 - 0.000434 lb/in³

@Pressure 14.69 psi,
Temperature 68.0 °F
BASF Basotect UL Foam
Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh..
Density 0.00400 - 0.0120 g/cc

@Pressure 0.1013 MPa,
Temperature 20.0 °C
0.000145 - 0.000434 lb/in³

@Pressure 14.69 psi,
Temperature 68.0 °F
BASF Basotect W Foam
Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh..
Density 0.00400 - 0.0120 g/cc

@Pressure 0.1013 MPa,
Temperature 20.0 °C
0.000145 - 0.000434 lb/in³

@Pressure 14.69 psi,
Temperature 68.0 °F
BASF Basotect TG Foam
Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh..