Teknor Apex Flexalloy® 9800-45 Polyvinyl Chloride Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 9800-45 Polyvinyl Chloride Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and Cable Applications, SealsForms-PelletsProcessing- Injection MoldingInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
23°C; ASTM D792
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 177 °C
30 g/10 min

@Load 11.0 lb,
Temperature 351 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
15 seconds; ASTM D2240
Tensile Strength, Yield 5.72 MPa
830 psi
ASTM D412
6.29 MPa
913 psi
110% Retention; Oil Immersion, ASTM #3 oil, 125°C, 7 days
Elongation at Break 262.8 %
262.8 %
73% Retention; Oil Immersion, ASTM #3 oil, 125°C, 7 Days
360 %
360 %
ASTM D412
Compression Set 36 %
36 %
158°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
>60 min.
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Descriptive Properties Value Comments
Swell 1.3%; Oil Immersion, ASTM #3 oil, 125°C, 7 days