Zeon Chemicals Nipol® 1082V Polyblend Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 1082V Polyblend Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is increased. Low temperature flexibility and resiliency are improved as butadiene content increases.Used for soft rolls and other low durometer goods. Contains 50 phr DIDP plasticizer.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Mooney Viscosity 30 - 45

@Temperature 100 °C
30 - 45

@Temperature 212 °F
(1+4)
Mechanical Properties Metric English Comments
100% Modulus 0.00740 - 0.0113 GPa
1.07 - 1.64 ksi
Descriptive Properties Value Comments
Bound ACN (%, acrylonitrile) 34
Type PB