Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Williams Advanced Alloys WS212 Solder

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS212 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 8.87 g/cc
0.320 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.4 MPa
6000 psi
Thermal Properties Metric English Comments
CTE, linear 23.6 µm/m-°C

@Temperature 20.0 °C
13.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 47.0 W/m-K
326 BTU-in/hr-ft²-°F
Melting Point 183 - 212 °C
361 - 414 °F
Solidus 183 °C
361 °F
Liquidus 212 °C
414 °F
Component Elements Properties Metric English Comments
Lead, Pb 50 %
50 %
Tin, Sn 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001578 ohm-cm
0.00001578 ohm-cm
Users viewing this material also viewed the following: