Williams Advanced Alloys WS174 Solder

Category Metal , Nonferrous Metal , Indium Alloy , Solder/Braze Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS174 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 8.19 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.8 MPa
3450 psi
Thermal Properties Metric English Comments
CTE, linear 28.0 µm/m-°C

@Temperature 20.0 °C
15.6 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 38.0 W/m-K
264 BTU-in/hr-ft²-°F
Melting Point 165 - 174 °C
329 - 345 °F
Solidus 165 °C
329 °F
Liquidus 174 °C
345 °F
Component Elements Properties Metric English Comments
Indium, In 70 %
70 %
Lead, Pb 30 %
30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001955 ohm-cm
0.00001955 ohm-cm