Wieland 1746 Wilaform Platinum

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer Wieland
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1746 Wilaform Platinum.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Platinum alloy particularly suitable for decoration castingApplications: casting, laminar decoration, tubingDental
Physical Properties Metric English Comments
Density 20.8 g/cc
0.751 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 135
135
HV5; glowed
Thermal Properties Metric English Comments
Melting Point 1750 - 1765 °C
3180 - 3209 °F
Solidus 1750 °C
3180 °F
Liquidus 1765 °C
3209 °F
Component Elements Properties Metric English Comments
Cobalt, Co 5.0 %
5.0 %
Platinum, Pt 95 %
95 %
Processing Properties Metric English Comments
Casting Temperature 1950 - 2150 °C
3540 - 3900 °F
Descriptive Properties Value Comments
Color platinum-white