Wieland 1401 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1401 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 13.9 g/cc
0.502 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 130
130
HV5; glowed
Tensile Strength, Ultimate 500 MPa
72500 psi
Elongation at Break 30 %
30 %
Thermal Properties Metric English Comments
Melting Point 850 - 880 °C
1560 - 1620 °F
Solidus 850 °C
1560 °F
Liquidus 880 °C
1620 °F
Component Elements Properties Metric English Comments
Copper, Cu 11.5 %
11.5 %
Gold, Au 58.5 %
58.5 %
Silver, Ag 30 %
30 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 980 - 1080 °C
1800 - 1980 °F
Descriptive Properties Value Comments
Color yellow