Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Westlake Plastics
Trade Name Propylux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux HS2 is produced from a FDA and USP Class VI approved homopolymer resin, and exhibits better heat and dimensional stability over Propylux HS. Recommended sterilization techniques for Propylux HS2 include steam autoclaving and cold sterilization.Applications Include:Provisional trialsCranio-maxillofacial traysSterilization tray componentsAdvantages of Medical Grade Propylux HS2:Excellent chemical resistanceLaser markableLot controlled and traceableLow moisture absorptionFDA resinSuperior dimensional stabilityInformation provided by Westlake Plastics Company.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Water Absorption 0.010 %
0.010 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength at Break 29.2 MPa
4230 psi
ASTM D638
Tensile Strength, Yield 34.3 MPa
4970 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
ASTM D638
Flexural Strength 64.6 MPa
9370 psi
ASTM D790
Flexural Modulus 2.27 GPa
329 ksi
ASTM D790
Compressive Yield Strength 47.4 MPa
6880 psi
ASTM D695
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 78.7 µm/m-°C
43.7 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.9 °C
201 °F
ASTM D648
Flammability, UL94 HB
HB