Westlake Plastics Clariflex® TFE/VF2/HFP

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer Westlake Plastics
Trade Name Clariflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Clariflex® TFE/VF2/HFP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Clariflex is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoro-propylene, and vinylidene fluoride. Notable properties include light transmission, chemical resistance and flame resistance. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Water Absorption 0.040 %
0.040 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Tensile Modulus 0.222 GPa
32.2 ksi
ASTM D638
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus 0.207 GPa
30.0 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 146 µm/m-°C

@Temperature 20.0 °C
81.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 166 °C
330 °F
ASTM D4591
Maximum Service Temperature, Air 149 °C
300 °F
Continuous Use
Deflection Temperature at 1.8 MPa (264 psi) 27.8 °C
82.0 °F
ASTM D648
Flammability, UL94 V-0
V-0
Oxygen Index 75 %
75 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Dielectric Constant 6.3

@Frequency 1000 Hz
6.3

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 10.6 kV/mm
270 kV/in
ASTM D149