Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake EB561 6.5% Ethylene Vinyl Acetate Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EB561 6.5% Ethylene Vinyl Acetate Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent sealability, excellent impact strength, good optics and enhanced stabilization.Application/UsesFrozen food packagingFresh food packagingIce bagsHeavy duty produce bagsFDA: This material complies with FDA regulations in 21 CFR, section 177.1350. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.929 g/cc
0.0336 lb/in³
ASTM D1505
Vinyl Acetate Content 6.5 %
6.5 %
Thickness 31.8 microns
1.25 mil
Melt Flow 0.55 g/10 min
0.55 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 380 %
380 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Dart Drop 18.9 g/micron
480 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 24.1 MPa
3500 psi
ASTM D882
Film Tensile Strength at Break, TD 25.5 MPa
3700 psi
ASTM D882
1% Secant Modulus, MD 103 MPa
15000 psi
ASTM D882
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 4.8 %
4.8 %
ASTM D1003
Gloss 74 %
74 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved